牌號
|
1.4123馬氏體耐腐蝕鋼
|
|
|
|
|
|
|
|
|
|
|
|
歐標鋼號
|
X40CrMoVN 16-2
|
|
|
|
|
|
|
|
|
|
|
|
對應標準
|
EN 10088-1-2005
|
|
|
|
|
|
|
|
|
|
|
|
不銹鋼 第1部分:不銹鋼的清單
|
|
|
|
|
|
|
|
|
|
|
|
Staehle Stainless steels. Part 1:List of stainless steels
|
|
|
|
|
|
|
|
|
|
|
|
歸類
|
馬氏體不銹鋼
|
|
|
|
|
|
|
|
|
|
|
|
性能
|
耐腐蝕
|
|
|
|
|
|
|
|
|
|
|
|
標簽
|
馬氏體不銹鋼
|
|
|
|
|
|
|
|
|
|
|
|
密度
|
7.7 g/cm3
|
|
|
|
|
|
|
|
|
|
|
|
X40CrMoVN 16-2 化學元素成分含量(%)
|
|
|
|
|
|
|
|
|
|
|
|
|
成分
|
C ?
|
Si
|
Mn
|
P
|
S
|
Cr
|
Ni
|
Mo
|
N
|
V
|
|
|
最小值
|
0.35
|
-
|
-
|
-
|
-
|
14
|
-
|
1
|
0.1
|
-
|
|
|
最大值
|
0.5
|
1
|
1
|
0.04
|
0.015
|
16
|
0.5
|
2.5
|
0.3
|
1.5
|
|
|
① 未經買方同意,不得隨意向鋼中添加表中未列的元素,冶煉精加工除外。采取一切必要措施以防在廢鋼和生產原料中帶入這些元素,因為其會削弱鋼的機械性能,降低鋼的適用性。
|
|
|
|
|
|
|
|
|
|
|
|
|
? 在詢問和定購時可同意更嚴格的碳含量范圍。
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
物理性能
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
各溫度時彈性模量
|
20°C與各溫度間熱膨脹系數
|
熱導率
|
比熱容
|
電阻率
|
磁性
|
20°C
|
100°C
|
200°C
|
300°C
|
400°C
|
100°C
|
200°C
|
300°C
|
400°C
|
20°C
|
20°C
|
20°C
|
GPa
|
10-6 K-1
|
W/m.K
|
J/kg.K
|
Ω.mm2/m
|
195
|
188
|
182
|
177
|
-
|
10.4
|
10.6
|
10.8
|
11.1
|
24
|
430
|
0.8
|
有
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|