INCOFLUXR 4 埋弧焊劑
INCOFLUX 4 埋弧焊劑是一種燒結焊劑,設計與INCONEL 82焊絲匹配使用,INCONEL 82焊絲是一種含鉻20%的高鎳合金。這種焊劑的典型應用是INCONEL600/601合金、INCOLOY 800合金相互之間及它們與鐵素體金屬材料之間的開坡口焊接。這種焊絲和焊劑的匹配尤其適用于碳鋼與不銹鋼之間的焊接,因為其熔敷金屬具有最優的熱脹系數。這種焊劑的另一個主要應用是與INCONEL 82填充金屬相匹配,在碳鋼表面堆焊形成耐蝕耐氧化層。
儲藏和干燥條件 焊劑密封在未開啟的容器中可以無限期保存。如果焊劑暴露于潮濕環境中,可以在500oF保溫烘干2小時或600oF保溫烘干1小時后使用。
The INCOFLUX 4 submerged arc welding agent is a sintering flux, which is designed to be used with INCONEL 82 welding wire. INCONEL 82 welding wire is a high nickel alloy with 20 % chromium. The typical application of this flux is INCONEL600/601 alloy, INCOLOY 800 alloy, and their welding between them and ferritic metal materials. This kind of wire and flux matching is especially suitable for welding between carbon steel and stainless steel because of its optimal thermal expansion coefficient. Another major application of this flux is the matching of the INCONEL 82 filler metal to the surface of carbon steel. Welding parameters: open groove welding or surfacing: apply DCEP current and narrow weld path Electrode dry extension flux layer thickness of wire diameter current/ampere voltage/v welding speed electrode 0.062 in 1.6 mm 240-290 30-33 8-11 in/min In 200-280 - mm/min 7/8-1 1/2-1 in 22 to 25 mm 13 to 25 mm 0.093 in 2.4mm 250-300 30-33 8-11 in/min In 200-280 - mm/min 7/8-1 22-25 mm 3/4-5/4 in 19 to 32 mm Electrode swing surfacing welding: the use of DCEN current mode, when the wire diameter is 0.062 in, the oscillation frequency is 50-70 weeks/min; When the wire diameter is 0.093 in, the oscillation frequency is 35-60 weeks/min 0.062 in 1.6 mm 240-2632-34 4 in/min 100 mm/min in 7/8-1 1/2-1 in 22 to 25 mm 13 to 25 mm 0.093 in 2.4mm 300-400 34-37 4 in/min 100 mm/min in 7/8-1 22-25 mm 3/4-5/4 in 19 to 32 mm Storage and drying conditions The flux seals can be kept indefinitely in unopened containers. If the solder is exposed to wet conditions, it can be used after an hour of thermal insulation drying for 2 hours or 600oF. Flux particle size Taylor's mesh: 10 times 100 packaging The barrel cover is covered with a 60 - pound polyethylene barrel sealed with rubber gasketINCOFLUXR 4 埋弧焊劑與INCONEL 82焊絲匹配INCOFLUXR 4 埋弧焊劑與INCONEL 82焊絲匹配INCOFLUXR 4 埋弧焊劑與INCONEL 82焊絲匹配INCOFLUXR 4 埋弧焊劑與INCONEL 82焊絲匹配INCOFLUXR 4 埋弧焊劑與INCONEL 82焊絲匹配 |
版權聲明:以上所展示的信息由會員自行提供,內容的真實性、準確性和合法性由發布會員負責。機電之家對此不承擔任何責任。 友情提醒:為規避購買風險,建議您在購買相關產品前務必確認供應商資質及產品質量。 |